Slump Retention and 7- and 28-Day Strength of M40 Concrete with GGBS, Fly Ash and a Combined GGBS–Fly Ash Binder at Constant Water and Binder Contents

Syed Shaheem Muzafer *

Department of Civil Engineering, Universal Group of Institutions, I.K. Gujral Punjab Technical University Jalandhar, Punjab, India.

Mandeep Saini

Department of Civil Engineering, Universal Group of Institutions, I.K. Gujral Punjab Technical University Jalandhar, Punjab, India.

*Author to whom correspondence should be addressed.


Abstract

Partial replacement of ordinary Portland cement (OPC) with fly ash or ground granulated blast furnace slag (GGBS) is widely reported to improve workability and to slow early strength gain, but the replacement levels recommended in the literature were obtained for different grades, binder contents and test ages, and few studies report the slump remaining at the time of placement. This paper reports a controlled comparison of four M40 concretes that shared the same total binder content (440 kg/m3) and the same design free-water content (162.8 kg/m3, water-to-binder ratio 0.37) and differed only in the binder: OPC alone (Mix 1), 45% GGBS (Mix 2), 18.18% fly ash (Mix 3) and 35% GGBS with 15% fly ash (Mix 4). The mixes were proportioned by the absolute volume method of IS 10262:2019 with a polycarboxylate superplasticiser. Slump was measured immediately after mixing and after 30 minutes; 150 mm cubes, 150 × 150 × 700 mm beams and 150 × 300 mm cylinders were water-cured and tested at 7 and 28 days, with two specimens per condition. All three blends were more workable than the control: initial slumps were 145, 165, 165 and 180 mm and 30-minute slumps were 100, 130, 110 and 120 mm for Mixes 1 to 4, so the slag mix retained the most slump and the fly ash mix lost the most. The control was strongest at both ages in all three tests. At 28 days the cube strengths were 55.42, 53.54, 50.95 and 50.01 N/mm2, all above the 48.3 N/mm2 target mean; flexural strengths were 5.13 to 4.85 N/mm2 and split tensile strengths 2.85 to 2.75 N/mm2. Every reduction relative to the control was smaller at 28 days than at 7 days, and the blends gained 32 to 41% in compressive strength between the two ages against 24% for the control. Mix 2 came within 3.4%, 1.6% and 1.1% of the control in the three 28-day tests while displacing 198 kg/m3 of OPC; Mix 4 displaced 220 kg/m3 and still exceeded the M40 target. The results are specific to these materials and proportions and rest on two specimens per condition.

Keywords: Blended cement, fly ash, ground granulated blast furnace slag, slump loss, compressive strength, flexural strength, split tensile strength, M40 concrete


How to Cite

Muzafer, Syed Shaheem, and Mandeep Saini. 2026. “Slump Retention and 7- and 28-Day Strength of M40 Concrete With GGBS, Fly Ash and a Combined GGBS–Fly Ash Binder at Constant Water and Binder Contents”. Journal of Engineering Research and Reports 28 (12):1-11. https://doi.org/10.9734/jerr/2026/v28i122058.

Downloads

Download data is not yet available.